Argeloy NP Apex
Non-Precious Alloys
Color | WHITE |
Type | 3 |
ADA Class | Predominantly Base (PB) |
Application
![]() ![]() |
Processing | |
---|---|
Investment | Phosphate Bonded |
Crucible | Quartz or Zircon |
Degassing Temp C | 650-1040 |
Oxidation Procedure | Hold 0 Min With Vacuum, Remove Oxide |
Solder & Laser Wires | |
---|---|
PreSolder | P, NP, Flux-N-SOL |
PostSolder | LO, R |
Laser Wire | LWNPNI |
Physical Properties | |
---|---|
VHN After Firing | 240 |
VHN Soft | |
VHN Hard | |
Proof Stress Soft MPa | 350 |
Proof Stress Hard MPa | |
Tensile Strength Soft MPa | 1138 |
Tensile Strength Hard MPa | |
Elongation Soft | 12 |
Elongation Hard | |
Elastic Modulus GPa |
Composition | |
---|---|
Nickel (Ni) | 64.0 |
Chromium (Cr) | 24.0 |
Molybdenum (Mo) | 9.0 |
Silicon (Si) | 3.0 |
Thermal Properties | |
---|---|
Melting Range C | 1230-1320 |
Casting Temp C | 1450 |
Density g/cc | 8.2 |
Expansion at 500C | 14.3 |
Expansion at 600C | 14.6 |
Burnout Temp C | 870 |